Thermal analyses of NaNO3-RbNO3 pseudo-binary system-differential scanning calorimetry

A.Sadananda chary, M.V.Madhava Rao, S.Narender Reddy


The differential scanning calorimetry (DSC) in NaxRb1-xNO3 pseudo-binary systemare presented by varying x from0 to 1. The formation of an intermediate compound and its effect on the phase transitions of RbNO3 is explained in terms of redistribution of energies involved in various transitions. Corresponding phase diagramis constructed. DSC peak at about 173 C with eutectic composition 0.46 (Na mole fraction) has been attributed to the formation of a congruently melting compound NaRb(NO3)2. X-Ray Diffracto grams (XRD) indicate the formation of this newcompound. DSCpeak corresponding to the melting of this compound and XRD lines related to this compound are found to grow with x until it reaches the eutectic composition.


免责声明: 此摘要通过人工智能工具翻译,尚未经过审核或验证

索引于

  • 中国社会科学院
  • 谷歌学术
  • 打开 J 门
  • 中国知网(CNKI)
  • 引用因子
  • 宇宙IF
  • 研究期刊索引目录 (DRJI)
  • 秘密搜索引擎实验室
  • 学术文章影响因子(SAJI))

查看更多

期刊国际标准号

期刊 h 指数

Flyer