Use of electrochemical measurements and surface analysis for the evaluation of the protective properties of 3-phenyl-1,2,4-tiazole-5-thione formulation of metallic cultural heritage

Ahmed Dermaj, Driss Chebabe*, Najat Hajjaji, Vincent Vivier


In this work a formulation of a new organic compound, namely 3-phenyl- 1.2.4-triazole-5-thione, was tested as a bronze corrosion inhibitor. This formulation (FPTS) has proven to be environmentally friendly, cheap and easy to use. The inhibitory effect of this formulation has been studied on commercial bronze (B66)with chemical composition,metallurgical features and micro-chemical structure similar to that of the ancient alloys installed in museumof Rabat (capital ofMorocco) near the atlantic ocean, in order to be successfully employed and used for testing corrosion inhibitor validating cleaning and conservation techniques. Electrochemical impedance spectroscopy (EIS), potentiodynamic polarization, Scanning Electron Microscopy coupled with chemical analysis (SEM and EDAX) and X-ray photoelectron Spectroscopy were used to study the inhibition action of FPTS in 3% NaCl. The obtained results show that the FPTS formulation has a significant effect against corrosion of B66 bronze in 3% NaCl solution, reaching an efficiency of 99% at 5.10-3M. This result encouraged us to test this formulation on real archaeological objects. The evaluation of the protective effect of FPTS on archaeological bronzes shows that it provides good protection of the Bronze artefacts against atmospheric corrosion for a long duration of exposure.


免责声明: 此摘要通过人工智能工具翻译,尚未经过审核或验证

索引于

  • 中国社会科学院
  • 谷歌学术
  • 打开 J 门
  • 中国知网(CNKI)
  • 引用因子
  • 宇宙IF
  • 研究期刊索引目录 (DRJI)
  • 秘密搜索引擎实验室
  • 学术文章影响因子(SAJI))
  • ICMJE

查看更多

期刊国际标准号

期刊 h 指数

Flyer